EN10025-3 steel plate S460N shall be rolled according to the below table of chemical composition.The limits applicable for the product analysis of structural steel plate s460n are given in the below table. The manufacturer shall inform the purchaser at the time of the enquiry and order which of the alloying elements appropriate to the steel grade required will be deliberately added to the material to be delivered. The product analysis shall be carried out when specified at the time of the order.Normalized heat treatment should be done for steel sheet S460N.
Technical Requirements & Additional Services:
Low temperature impacting test
Rolling under standard NACE MR-0175 (HIC+SSCC)
Ultrasonic test under EN 10160,ASTM A435,A577,A578
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
Shot blasting and Painting,Cutting and welding as per end user s demands
Mechnical property for S460N Structural steel:
Thickness (mm) | ||||||||
S460N | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 460 | 440 | 430 | 410 | 400 | 380 | 370 | 370 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 540-720 | 530-710 | 530-710 |
Main chemical elements composition of S460N | ||||||
C | Si | Mn | P | S | Nb | V |
0.20 | 0.60 | 1.00-1.70 | 0.030 | 0.025 | 0.05 | 0.20 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.80 | 0.10 | 0.55 | 0.025 |